What is HP Multi Jet Fusion? A plain guide for engineers in India
How HP Multi Jet Fusion builds nylon parts layer by layer, what the agents do, which materials it uses and when it is the right process for your part.
HP Multi Jet Fusion (MJF) is a powder bed 3D printing process that builds nylon parts by printing liquid agents onto a thin layer of powder and then heating the whole layer at once. The result is strong, detailed functional parts with no support structures, made quickly enough to compete with tooling at low and medium volumes.
This guide explains what happens inside the machine, what the process is good at, where it falls short, and what an engineer should know before sending a first file.
How Multi Jet Fusion works
HP describes MJF as a mix of two older ideas: powder bed fusion, where heat fuses plastic powder, and binder jetting, where print heads place liquid on a powder bed. Instead of a laser tracing each part point by point, MJF treats the whole layer like a sheet of paper in an inkjet printer.
Each layer goes through the same short cycle:
- Recoat. A thin, even layer of nylon powder is spread across a preheated build bed.
- Print agents. Inkjet print heads pass over the bed and jet two liquids. A fusing agent goes wherever the part should be solid. A detailing agent goes along the edges of the part.
- Fuse. An energy source passes over the bed. Additive Manufacturing Media describes this as infrared light. Powder carrying the fusing agent absorbs the heat and melts. Untreated powder stays loose.
- Repeat. The bed drops by one layer and the cycle starts again.
When the build finishes, the build unit and the block of powder inside it must cool before the parts can be taken out. The loose powder is removed by vacuum, the parts are cleaned, usually by blasting, and unused powder is collected for the next build.
Because the print heads cover the full width of the bed in one pass, every layer takes about the same time whether it holds one part or fifty. That is why MJF rewards full builds.
What the two agents do
The fusing agent is the simpler of the two. It is a heat-absorbing ink that tells the powder where to melt.
The detailing agent matters more than its name suggests. Melting nylon tends to spread heat into the powder around it, which would blur edges and let loose powder stick to the part. The detailing agent works against this at the boundary, which keeps edges sharp and stops the melt from bleeding outwards. HP credits it with the small holes, fine lattices and surface textures the process can hold.
HP calls each printed point a voxel, the 3D version of a pixel. Its 2017 technical note says the process can address up to 1,200 voxels per linear inch in each layer. That is the print head's addressing limit, not the accuracy you should expect on a finished part. Real dimensional accuracy depends on part size, geometry and orientation.
Layers, build size and speed
Layer thickness on MJF machines is usually around 0.08 mm. HP's 2017 note gives a range of 70 to 120 microns for the Jet Fusion 4200, and the University of Technology Sydney lists about 80 microns on its Jet Fusion 5200. Thin layers are part of why MJF parts show fine text and crisp ribs.
The same university lists a build volume of 380 × 280 × 380 mm, which matches the MJF build volume we run at our Hyderabad unit. Parts can be stacked through the full height of that volume because the loose powder holds them in place. Nothing needs supports, so there are no support marks to remove and internal channels print cleanly.
Materials and part properties
Most MJF work is done in PA 12, a nylon that is tough, stiff and stable. HP's PA 12 grade is sold as HP 3D High Reusability PA 12. Its material listing says parts resist oils, greases, aliphatic hydrocarbons and alkalies, and can be watertight without extra post-processing. HP's range also includes PA 11 and a glass-bead filled PA 12 (PA 12 GB), and several chemical companies develop powders for the platform.
A few properties matter most to engineers:
- Even strength in all directions. HP and the University of Technology Sydney both describe MJF parts as close to isotropic. This is the main difference from FDM, where parts are weakest between layers.
- Consistency. Additive Manufacturing Media notes that MJF parts tend to warp less than SLS parts and have more consistent mechanical properties, because the powder supports each part from below.
- Powder reuse. HP rates its PA 12 at 80% surplus powder reusability, which cuts waste and cost per part.
For full PA 12 values, including tensile strength and heat deflection, see our PA 12 material page.
MJF compared with SLS and FDM
Engineers often weigh MJF against selective laser sintering (SLS), the other main nylon powder process, and against FDM.
| MJF | SLS | FDM | |
|---|---|---|---|
| How a layer is made | Agents jetted, whole layer heated | Laser traces each part | Nozzle draws each line |
| Supports | None | None | Needed under overhangs |
| Strength across layers | Close to isotropic | Strong, functional parts | Weakest between layers |
| Best for | Functional parts and batches | Functional nylon parts | Large, simple, low-cost parts |
| Surface | Even, fine-grained matte | Matte | Visible layer lines |
HP's own comparison says both MJF and SLS make strong functional parts. HP's case for MJF is predictable print times and fine detail from the detailing agent. SLS dates back to the 1980s and is also offered in filled nylons, such as glass and carbon fibre grades. For a detailed look at the FDM side, read our MJF or FDM guide.
Where MJF fits, and where it does not
MJF is a good choice when:
- The part has to work: snap-fits, hinges, brackets, housings, ducts and mounts.
- You need from tens to hundreds of identical parts without paying for a mould.
- The design has internal channels, lattices or assemblies that cannot be machined.
- Strength in every direction matters more than surface gloss.
It is a weaker choice when:
- The part is large and mostly solid. The University of Technology Sydney notes that large solid or fully enclosed hollow parts can be costly, because they use a lot of material and heat.
- You need a smooth, glossy or clear surface straight off the machine. Raw MJF parts are grey and slightly grainy, so they need dyeing or painting for a cosmetic finish.
- The part is bigger than the build volume and cannot be split.
HP lists drones, automotive, industrial equipment, healthcare and consumer electronics among the main users of the process. In India, that maps closely to the defence, aerospace, drone and robotics teams that need strong parts in small batches.
Frequently asked questions
Is MJF the same as SLS? No. Both fuse nylon powder without supports, but SLS uses a laser to trace each part, while MJF jets agents onto the powder and heats the whole layer at once.
Are MJF parts strong enough for end use? Yes, for many uses. PA 12 MJF parts are tough, close to isotropic and resistant to oils and many chemicals. Check the loads and temperatures against the material data before using them in a critical part.
Why are raw MJF parts grey? Natural grey is how fused PA 12 comes out of the machine. Dyeing gives a uniform black, and painting gives other colours.
Do I need to design differently for MJF? A little. Keep walls at about 1 mm or more, leave gaps between moving parts and hollow thick sections. Our MJF design checklist covers the rules.
How do I get an MJF quote in Hyderabad? Upload STEP or STL files on our quote page. We reply within 1 to 5 hours on working days, with no minimum order.
Sources
- MJF vs SLS: what is the difference? (HP)
- Introduction to 3D printing processes (HP)
- The HP Multi Jet Fusion voxel: building 3D objects with controllable properties (HP technical note, 2017)
- HP Multi Jet Fusion 3D printing technology (HP)
- AM 101: Multi Jet Fusion (MJF) (Additive Manufacturing Media)
- Multi Jet Fusion 3D printing (UTS ProtoSpace, University of Technology Sydney)
- HP 3D High Reusability PA 12 (UL Prospector material listing)